Views: 0 Author: Site Editor Publish Time: 2026-10-30 Origin: Site
Why must it be?
The output power of a single optical fiber cannot be increased infinitely. Nonlinear effects such as thermal damage, stimulated Raman scattering (SRS), end face damage and thermal lenching effect jointly draw a "physical ceiling" - the power limit of single-mode wide-spectrum fiber lasers provided by Dawson et al. at Livermore National Laboratory in the United States is approximately 36.6 kW. However, the brightness and power that a single semiconductor pump module can provide are also limited. To power a fiber laser of several kilowatts or even tens of thousands of watts, it is necessary to "parallel" a dozen pump lights.
The beam combiner is a passive coupling device with an all-fiber structure, featuring no glue, no mechanical moving parts, and no free space alignment. It uses a fused cone to "lengthen" multiple input optical fibers into a single output optical fiber. According to function, it can be divided into two major categories:
• Pump Combiner: Injects multiple pump lights into the inner cladding of the double-clad gain fiber to provide energy for laser amplification.
• Signal & Power Combiner: It combines multiple already amplified lasers into a single output fiber for direct power expansion. In all-fiber structure lasers and amplifiers, gain fibers, high-brightness pump sources and pump combiners are collectively known as the three key components. Among them, the power characteristics of the beam combiner directly affect the final output of the entire machine. It can be said that the laser can output as many watts as the beam combiner can withstand.
Three unbreakable rules
Luminance conservation
The pump combinator brings a large amount of low-brightness pump light into an optical fiber, adding up the power without increasing the brightness. This is especially true for signal power combiners - power can be linearly superimposed, and beam quality (brightness) usually does not increase but decreases or is basically conserved.
Adiabatic tapering
The core process of the Bundle binder is Fused Biconical Taper (FBT/Tapered Fiber Bundle, TFB). During the tapering process, the diameter of the optical fiber gradually decreases, and the mode field, numerical aperture, and power density change accordingly: the thinner the waist region, the stronger the optical field constraint, and the more conducive it is to mode coupling and energy merging. The key requirement is "adiabatic" - the rate of change of the waveguide structure must be much lower than the energy exchange rate between modes, so that the light field energy only transfers orderly between modes and does not radiate outward.
Mold field matching and fusion splicing
After the cone waist cutting, it needs to be spliced with the output optical fiber. The loss mainly comes from three parts: the mismatch of the mode field diameter, the lateral offset Δ, and the angular deviation θ. In engineering, this loss is reduced by "pre-pulling the cone output optical fiber - matching the waist diameter - actively aligning and splicing", and at the same time, the output end is cut at an 8° Angle to suppress the return light coupling back to the pump source.
Shinho S-37 series offer a good mold field mathing and high quality splicing to achieve best IL for the combiner.